Nonlinear Optical Properties Of B203-Based Glasses: M20-B203 (M=Li, Na, K, Rb, Cs, And Ag) Binary Borate Glasses

The third order nonlinear optical susceptibilities x(3) of M20-B2O3- (M=Li, Na, K, Rb, Cs and Ag) binary borate glasses have been measured by the third harmonic generation (THG) method.