Nonlinear Optical Effects In Organically Doped Low Melting Glasses

Saturable absorption is described in a new family of nonlinear optical materials in which organic dopants are combined directly into a low melting glass

Author
P A Tick, D W Hall
Origin
Corning Glass Works
Journal Title
Diffusion And Defect Data 1987 53-54 179-188