Nonlinear Coefficient Of Optical Fibres At 1550Nm

A major revolution in lightwave transmission systems is ocurring with the advent of erbium-doped fibre amplifiers. They have allowed transmission over transoceanic distances without the need of electronic repeaters and enabled high speed, multiwavelentgh terrestrial transmission systems.

Author
V L Dasilva Et Al
Origin
Corning Inc, Usa
Journal Title
Corning Research 1997 95-99