Non-Newtonian Viscous Flow And Tensile Strength Of Silicate Glass At High Deformation Rates

The non-Newtonian behaviour of glass is discussed and an attempt is made to evaluate failure stress from the measured force and the observed failure cross-section.

Author
C Guillemet, R Gy
Origin
Saint-Gobain Recherche, Aubervilliers
Journal Title
Riv Staz Sper Vetro 1990 20 6 221-224
Sector
General
Class
G 556

Request article (free for British Glass members)

Non-Newtonian Viscous Flow And Tensile Strength Of Silicate Glass At High Deformation Rates
Riv Staz Sper Vetro 1990 20 6 221-224
G 556