Non-Contact Thickness Measurment And Dimension Check

VMA GmbH has been producing non-contact thickness measurement and dimension check systems for the glass industry for over 20 years. Products and services provided cover the fields of: float glass (TMF); container glass (TMC); tube glass (TC); and a recent addition, patterned (solar) glass sector. Together with partners in the field of strain and defect detection, VMA can provide comprehensive solutions, as explained in this article.