Nitrogen Cooling Boosts Glass Container Production

Trials on the use of AGA's process for cooling the air in the second stage of the blow-blow process with liquid nitrogen are reported. Tettauer AG are said to have achieved a 30% increase in production from an IS machine by this means.

Author
C D Norenberg
Origin
Industrial News Service - Ins Ab
Journal Title
Glass International 1988 September 58, 60
Sector
Container glass
Class
C 126