Nitrided Phosphate Glasses For Soldering Applications

Single and mixed alkali phosphate glasses have been nitrided in a dry ammonia atmosphere. Nitrogen incorporation kinetics were studied in order to fix the nitrogen content limits as function of temperature and time of thermal treatment. Thermal expansion coefficient, softening temperature and chemical durability of the nitrided glasses have been investigated with the aim of developing these glasses for sealing high and medium expansion coefficient materials.

Author
L Pascual & A Duran
Origin
Inst Ceramica Y Vidrio, Spain
Journal Title
Proc Xvii Icg Vol 5 Beijing 1995 157-162
Sector
Special Glass
Class
S 2166

Request article (free for British Glass members)

Nitrided Phosphate Glasses For Soldering Applications
Proc Xvii Icg Vol 5 Beijing 1995 157-162
S 2166
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.