Nippon Sheet Glass: Oil Prices Hit Operating Profit

Nippon Sheet Glass's group operating profit for fiscal 2005 fell 29.9% from the previous year to JPY8.429BN because of a rise in fuel costs reflecting higher crude oil prices, the firm said 31/05/06. Recurring profit for the year that ended in March/06 also fell 21.4% to JPY10.425BN. Higher fuel costs took a JPY3BN bite out of operating profit, according to officials. Meanwhile, the company's fiscal 2005 group sales increased 0.3% to JPY265BN on the back of steady sales of auto & flat glass for construction use outside Japan. Net profit rose 2.3% to JPY7.764BN as special profit increased JPY1.2BN from the previous year to JPY6.6BN thanks to a greater securities sales profit. NSG did not give earnings estimates for the current year end, as disclosure is restricted under British regulatory rules until the June/06 completion of its acquisition of Pilkington PLC.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline 07/06/06
Sector
Flat glass
Class
F 2037

Request article (free for British Glass members)

Nippon Sheet Glass: Oil Prices Hit Operating Profit
Glassonline 07/06/06
F 2037
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.