Nickel Sulphide Inclusions In Glass: An Example Of Microcracking Induced By A Volumetric Expanding Phase Change

Microcracking about inclusions of nickel sulphide in soda-lime glass has been studied. These cracks are nucleated by the volumetric expansion that accompanies the alpha-beta phase transformation in nickel sulphide. The a-phase is metastable and, upon transofrmation to the b-phase, is accompanied by a volumetric expansion of about 4%. The critical dimensions of the inclusion to initiate microcracking in an annealed specimen and to cause spontaneous fracture of a tempered plate are predicted.

Author
M V Swain
Origin
Saint Gobain Recherche, France
Journal Title
J Mat Sci 16 1981 151-158
Sector
Flat glass
Class
F 511

Request article (free for British Glass members)

Nickel Sulphide Inclusions In Glass: An Example Of Microcracking Induced By A Volumetric Expanding Phase Change
J Mat Sci 16 1981 151-158
F 511
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.