Nickel-Based Superalloys Suitable For Applicatins In The Glass Industry (In Czech)

Czech firm, Prvni Brnenska Strojirna Velka Bites has developed precise technology of casting parts suitable for glass industry applications. Structural materials are nickel-based superalloys 141, 141H, 141I, 145 and 2.4879. Mechanical properties and structural stability of these superalloys have been determined in the temperature range 20C to 1100C.

Author
Un-named
Origin
Unknown
Journal Title
Sklar Keram Cs 54 1-2 2004 4-6
Sector
General
Class
G 2845