Next Generation Emissions Control In A Single Step

Haldor Topsoe has recently supplied the glass manufacturing industry with "TopFrax" a catalytic ceramic filter, capable of trapping dust and controlling off-gases in a single step. According to the company, four glass manufacturers have already chosen this solution.