[New Zealand] Waste Glass Mountains Continue To Grow

The Packaging Council of New Zealand is trying to tackle the the mountains of container glass waste piling up around the country. John Webber, responsible for the packaging council's relationships with government said there was too much glass for the country's one bottle plant to consume & the situation was a lot more complicated than it appeared. He said researchers were searching "frantically" to find a use for the ever-growing mountains of glass. "To suggest that it cannot be used is wrong," he said. "It's serious, but the situation is not quite as black as it seems." One possibility is to crush the bottles to make aggregate for building materials. Over half of the bottled products consumed in New Zealand are imported, so having re-usable bottles would not be the answer, Mr Webber said. His group is pushing for a return to refundable deposits on bottles.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline 9/12/05
Sector
Container glass
Class
C 2866b

Request article (free for British Glass members)

[New Zealand] Waste Glass Mountains Continue To Grow
Glassonline 9/12/05
C 2866b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.