New Technologies For Oxygen Use In Glass Container Production: A Technical And Economical Overview

Oxy-fuel technology for glass melting was introduced at the beginning of the 90s. The main reason was the necessity to respect tighter limits for emissions of NOx in the atmosphere. This paper investigates why the high potential of this technology has been limited and the reasons for its partial success, then looks for new solutions.

Author
S De Sanctis
Origin
Sapio Spa, Italy
Journal Title
Int Glass Journal No 109 2000 32-36
Sector
Container glass
Class
C 1636

Request article (free for British Glass members)