New Smart Window Glass Changes From Clear To Dark In Nearly 3O Seconds

A Stanford University research team has created a new type of smart window that changes from transparent to dark in less than a minute. Self-tinting windows are not new, but this process is a significant improvement over existing technology, according to a Stanford News article. To read the article in full, please visit the above shown website.