A New Quantiative Method For Na Out Diffusion From Float Glass

This paper describes a new, fast, and dry method for sodium out diffusion analyses from a float glass. The method consists of the colouring level determination of previously calibrated electrochromic, EC, layer deposited on the glass surface. Integrated differential transmittance spectra of the glass/EC system measured before and after heat treatment is proportional to the forming colour of amount of Na diffused from glass into EC film.

Author
H Demiryont
Origin
Turkiye Sise Cam As, Istanbul
Journal Title
Proc Xviii Icg, San Francisco, Usa, July 1998 231-236
Sector
Special Glass
Class
S 1867

Request article (free for British Glass members)

A New Quantiative Method For Na Out Diffusion From Float Glass
Proc Xviii Icg, San Francisco, Usa, July 1998 231-236
S 1867