A New Quality Assurance Strategy By Using The Heye Process Control System For Lightweight Hap Forming Process

The Heye Process Control is a control and visualisation system which supports the forming process in the blank mould of an IS machine. Bottle defects arising during parison forming are recognised and rejected in connection with the E-Timing Hot End Ware Reject. Thereby, Process Control becomes a highly efficient inspection machine. This article describes the system and its operation as a process and quality control tool for the production of lightweight glass containers using the press and blow forming process.

Author
S Schwarzer
Origin
Heye Int, Germany
Journal Title
Int Glass Journal 129 2004 37-41
Sector
Container glass
Class
C 2392

Request article (free for British Glass members)

A New Quality Assurance Strategy By Using The Heye Process Control System For Lightweight Hap Forming Process
Int Glass Journal 129 2004 37-41
C 2392
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.