A New Method For Determining Fixed Viscosity Points Of Glasses

A method for obtaining viscosity-temperature data for glasses is provided on the basis of the characteristic points obtained by hot stage microscopy (HSM) in the range 6

Author
M J Pascual Et Al
Origin
Institute Ceramica Y Vidrio, Spain
Journal Title
Phys Chem Glasses 46 5 2005 512-520
Sector
Special Glass
Class
S 3047

Request article (free for British Glass members)

A New Method For Determining Fixed Viscosity Points Of Glasses
Phys Chem Glasses 46 5 2005 512-520
S 3047