New Method Designed For Collecting Hot End Cullet

A sluice system developed by Domglas and French Systems is claimed to provide for safer, more efficient handling of glass gobs.

Author
S B Parker, T G Dutaud
Origin
French Systems Inc, Domglas Inc.
Journal Title
Glass Industry February 1988 10-15