New Materials And Processes For Integrated Optics

Materials and processes for integrated optics are faced with increasing demands from telecommunications and instrumentation applications. Progress in three aspects of novel materials and processes are described: titanium-diffused sapphire waveguides and lasers, interferometric excimer laser ablation of waveguide gratings, and surface studies by waveguide surface plasmon resonance.