New Iso Standard Released For Solar Heat Gain

The International Organization for Standardization (ISO) has published a standard that specifies a method to measure the solar heat gain coefficient (SHGC) of complete doors and windows. ISO 19467:2017 is titled “Thermal Performance of Windows and Doors – Determination of solar heat gain coefficient using solar simulator.” According to the document, it is “designed to provide solar heat gain coefficient values by standardized measurement method and to enable a fair comparison of different products.” It specifies standardized apparatus and criteria, and the SHGC-measuring apparatus applied in it includes the solar simulator, climatic chamber and metering box. The document applies to doors and windows with various types of glazing, including systems that are single- or multi-glazed; with or without low-E coatings; and with spaces filled with air or gases. It also applies to doors and windows with opaque panels, as well as various types of frames, shading devices and solar fenestration systems – including building-integrated photovoltaics or building-integrated solar thermal collectors.

Author
Un-named
Origin
Unknown
Journal Title
www.Iso.org/Standard/64989.Html
Sector
Flat glass
Class
F 3996

Request article (free for British Glass members)

New Iso Standard Released For Solar Heat Gain
www.Iso.org/Standard/64989.Html
F 3996
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.