New Glass From Saint-Gobain

Saint-Gobain has introduced a new glass, Plantherm Total 1.3, the first single stock toughenable and durable high performance low-emissivity coated glass. It will be made on the UK's first magnetron coater, installed at the firm's factory at Eggborough. (whole item)