New Glass Packaging For Foodstuffs (German)

The physical properties and production methods for vacuum deposited silica coatings are discussed.

Author
T Krug, K Rubsam
Origin
Unknown
Journal Title
Neue Verpack 1991 44 5 46 - 48
Sector
Container glass
Class
C 441