A New Family Of Lead-Bismuthate Glass With A Large Transmitting Window

New glasses with high Li2O content have been obtained in the system Li20-Bi203-PbO. The role of the different components in the glass formation has been explored from the density and thermal measurements. A wide transmitting window having sharp cut-off in both ultraviolet-visible (UV-VIS) and Infrared (IR) regions for almost all compositions of these glasses has been observed, making them an appealing candidate for different spectral devices.

Author
A Pan & A Ghosh
Origin
Indian Assoc Cult Science, Calcutta
Journal Title
J Non-Cryst Solids 271 2000 157-161
Sector
Special Glass
Class
S 2619

Request article (free for British Glass members)

A New Family Of Lead-Bismuthate Glass With A Large Transmitting Window
J Non-Cryst Solids 271 2000 157-161
S 2619
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.