A New Equation Describing The Temperature Dependence Of The Electrical Resistivity Of Alkali Containing Silicate Melts

A new two parameter empirical equation describing the temperature dependence of the electrical Resistivity of glass forming melts is proposed in this article.

Author
A I Priven
Origin
Scite Ltd, Russia
Journal Title
Glass Technology 46 3 2005 263-270