New Developments From Weigand

Through an R&D partnership Wiegand has developed a coating process for glass containers. The container is coated with a 0.005 mm thin polymer & its internal pressure strength is increased by 50 %. Furthermore, with this coating, it is also possible to reduce the bottle weight by up to 30 %. By colouring the polymer, it is possible to produce the bottles in the desired colour. Also frosted effects can now be accomplished economically & in an environmentally friendly way. Also, Wiegand modified the cold-end surface treatment by coating & spraying the bottle after the lehr, therefore giving the surface a higher scratch resistance. Scuffing marks are minimized. This process has been patented.

Author
Un-named
Origin
Unknown
Journal Title
Weigand'S Website: www.Wiegand-Glas.De/English/Neuent.Htm
Sector
Container glass
Class
C 2775

Request article (free for British Glass members)

New Developments From Weigand
Weigand'S Website: www.Wiegand-Glas.De/English/Neuent.Htm
C 2775
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.