New Developments In Coatings

In this paper the author explores the growth of organic and UV technologies for the glassmaking sector looking at applications, coating requirements, coating processes, adhesion, factors affecting adhesion and lastly, UV curing lacquer.

Author
R Mckelvie
Origin
Schloetter Co Ltd, Uk
Journal Title
Glass Int Nov-Dec 2004 16, 18
Sector
General
Class
G 2884

Request article (free for British Glass members)

New Developments In Coatings
Glass Int Nov-Dec 2004 16, 18
G 2884