Network Glass Structure: A Neutron Scattering Study

An account is given of recent neutron diffraction and inelastic scattering studies of a number of different network glass-forming systems, using a combination of steady-state reactor and pulsed neutron sources. Both oxide and chalcogenide systems have been investigated and the interrelationship between their various network structures are discussed. The samples studied by diffraction include single component glasses and binary systems, consisting of a network modifier plus a network former , and the data have been extended to high values of the scattering vector, Q, to achieve high real space resolution. For a copy of the article please email: [email protected]

Author
A C Wright Et Al
Origin
Reading University, Uk
Journal Title
2002 Glass Odyssey 6Th Esg Conference Abstracts 16
Sector
Special Glass
Class
S 2793

Request article (free for British Glass members)

Network Glass Structure: A Neutron Scattering Study
2002 Glass Odyssey 6Th Esg Conference Abstracts 16
S 2793
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.