Nature Of Alumina In Phosphate Glass: 1, Properties Of Sodium Aluminophosphate Glass

The properties and structures of three additional series of sodium aluminophosphate glass are examined.

Author
R K Brow
Origin
Sandia National Labs, Usa
Journal Title
J Am Ceram Soc 76 4 1993 913-918
Sector
Special Glass
Class
S 720

Request article (free for British Glass members)

Nature Of Alumina In Phosphate Glass: 1, Properties Of Sodium Aluminophosphate Glass
J Am Ceram Soc 76 4 1993 913-918
S 720