Nanophase Ceramics For Improved Drug Delivery

After a decade of R&D, nanotechnology has reshaped the traditional thinking of using ceramics for drug delivery. Although drug delivery has been a polymer-dominated field, the blossoming of nanotechnology means that ceramic materials are now showing much promise for numerous drug delivery applications. Typically, nanotechnology is defined as the use of materials and systems whose structures and components exhibit novel and significantly changed properties when control is gained at the nanoscale. For ceramics, this means fabricating ceramics whose grain or particle sizes are within the range 1nm to 100nm.Nanophase ceramics already have been widely used in a broad spectrum of biomedical applications, and now drug delivery is one of the fastest emerging and developing arenas for nano-ceramics, drawing increasing attention over the past few years, as explained here.

Author
L Yang Et Al
Origin
Unknown
Journal Title
Am Ceram Soc Bull 89 2 2010 24-30
Sector
Special Glass
Class
S 3573

Request article (free for British Glass members)

Nanophase Ceramics For Improved Drug Delivery
Am Ceram Soc Bull 89 2 2010 24-30
S 3573
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.