Nanometer-Tall Cones Provide Antireflective Properties, Eliminate Glare

Researchers at the Centre for Functional Nanomaterials at Brookhaven National Laboratory (Upton, New York) have found a way to reduce the reflection of sunlight on glass by etching tiny nanometer-sized cones onto the glass's surface -making the glass virtually invisible. the cones have the effect of making the refractive index change gradually from that of air to that of glass, thereby avoiding reflections, according to a news release.

Author
Un-named
Origin
Unknown
Journal Title
Https://www.Bnl.Gov/Cfn/Research/Highlights/News.Php?A=212634
Sector
News Items
Class
N 3887

Request article (free for British Glass members)

Nanometer-Tall Cones Provide Antireflective Properties, Eliminate Glare
Https://www.Bnl.Gov/Cfn/Research/Highlights/News.Php?A=212634
N 3887
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.