Nano-Mechanical Properties Of Hydroxyapatite Coatings With A Focus On The Single Solidified Droplet

Hydroxyapatite (HAp) is a common implant material choice for orthopaedic implants and is mostly used as a coating to improve the biocompatibility of implants and stimulate tissue growth. This is a desirable material for implants, but the thermal instability requires strict control of the processing conditions to produce a crystalline coating. A coating with well molten particles has been produced from flattened solidified droplets. This development has allowed further investigation of the coating surface with nanoindentation, profilometry and electron microscopy. Instrumented i indentation testing, also known as depth-sensing indentation or nanoindentation, was used to gather information on the hardness and elastic modulus. It was found that the surface topography can lead to elevated values of the hardness and elastic modulus.

Author
K A Goss & S Saber-Samandari
Origin
University Melbourne, Australia
Journal Title
J Aust Ceram Soc 43 2 2007 98-101
Sector
Special Glass
Class
S 3255

Request article (free for British Glass members)

Nano-Mechanical Properties Of Hydroxyapatite Coatings With A Focus On The Single Solidified Droplet
J Aust Ceram Soc 43 2 2007 98-101
S 3255
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.