Nampak Invests Zar 1.6/Bn In Beverage Packaging

At its annual general meeting on 8 February, Nampak, Africa’s largest packaging company, announced that it is investing ZAR 1.6/BN in two of its core businesses which produce bottles and cans for the growing beverage market. The first project will see the company invest almost ZAR 1/BN in an additional furnace at its glass bottle business based at Roodekop, Germiston. This business already has two furnaces and a third furnace will improve overall manufacturing efficiencies and enable it to supply a broader range of bottles. Sales of the additional production have already been contracted to key customers. The second project is an investment of almost ZAR 600M to add aluminium beverage can capacity and convert existing lines from tinplate to aluminium. A new high speed line is being installed at the Springs plant for commissioning in May 2013 and will be followed by the conversion of the other existing lines. Sales have been secured through long-term supply contracts with major customers. Aluminium cans are fully recyclable so there will also be environmental benefits. Speaking at the meeting, Nampak’s chairman Tito Mboweni said: “These two projects strengthen our position in the beverage can and glass packaging sectors in South Africa and show our commitment to growing the South African economy.”

Author
Un-named
Origin
Unknown
Journal Title
www.Glassonline.com 14 Feb/2013
Sector
Container glass
Class
C 4814

Request article (free for British Glass members)

Nampak Invests Zar 1.6/Bn In Beverage Packaging
www.Glassonline.com 14 Feb/2013
C 4814
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.