Multicomponent Gas Bubbles. Part 2. Bubble Dynamics

The growth of rising gas bubbles in soda-lime glass melts is analysed by means of a lumped parameter which accounts for the surface tension. The calculations indicated that for melt temperatures above 1400 degrees C gas bubbles migrate to the surface but for lower temperatures mass transfer affects bubble dynamics and refining agents may be needed to cause bubble dissolution or growth by chemical reaction.

Author
J I Ramos
Origin
Unknown
Journal Title
J Non-Equilib Thermodyn 1988 13 2 107-113
Sector
General
Class
G 218