A Multi-Method Characterization Of Borosilicate Glasses Doped With 1 Up To 10 Mol% Fe, Ti And Sb

The model glasses NBS1 and NBS2 are sodium borosilicate glasses of high intrinsic UV transmission. Although both glasses have an Si02 content of 74 mol%, they possess different matrix structures due to varied Na20/B203 ratios. Nonbridging oxygens occur in the NBS1 but not in the NBS2 glass. Fe, Ti and Sb oxides were added at concentrations of 1 and 10 mol% to study valence, coordination and site distribution. XANES, Mossbauer, optical absorption, photoluminescence and EPR spectroscopy provided an insight into the structures and near range environments of the dopants. Large differences were found for the two Fe doped glasses. The presence of nonbridging oxygens in NBS1 glass leads to a higher solubility of the Fe ions and a higher ratio of tet

Author
A Schutz Et Al
Origin
Otto Schott Inst, Jena, Germany
Journal Title
Glass Sci Technol 77 6 2004 295-305
Sector
Special Glass
Class
S 2899

Request article (free for British Glass members)

A Multi-Method Characterization Of Borosilicate Glasses Doped With 1 Up To 10 Mol% Fe, Ti And Sb
Glass Sci Technol 77 6 2004 295-305
S 2899
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.