Multi-Dimensional Inspection Assures Coated Glass Quality

This article describes the benefits of a fully automated optical inspection system for coated glass. The system replaces operators with an easy, efficient and economic set-up for excellent defect detection and exact classification of coating and other irregularities in the surface over the entire glass.