Msc: Improving The Glass Container Forming Process

MSC's I-CARE system is made up of: One (or two) high resolution cameras installed alongside the conveyor just after the forming machine, equipped with a cooling system adapted to the high temperatures common at this point in the line. Their size is another of the system's features, around 25cm wide, taking up very little space alongside the conveyor, making it possible to position them easily in confined spaces; An air-conditioned electronic data processing unit connected to the camera by a fibre-optic cable long enough to install the camera up to 50 metres away & accommodate any line configuration & operating mode. The unit features a screen for displaying all the information operators will need to take immediate action on the forming machine; and, an Ethernet-connected remote unit for monitoring one or more process units (eg a furnace with several lines).

Author
G Lecat
Origin
Msc, France
Journal Title
Gmpa 1/2006 65-67
Sector
Container glass
Class
C 2948

Request article (free for British Glass members)

Msc: Improving The Glass Container Forming Process
Gmpa 1/2006 65-67
C 2948
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.