Mouldable Refractory Sheet

Zircar Refractory Composites Inc, Florida, USA, has introduced the refractory sheet type RS-A Moldable. This is a tough ceramic fibre reinforced insulation, containing no asbestos and ideally suited for a wide range of high temperature, high thermal shock applications. It is a wet blanket that can easily be formed into a wide variety of simple and complex shapes. Drying results in a strong rigid shape that can be wet again to restore the original flexibility. Firing irreversibly removes the flexibility, leaving it unaffected by moisture. The product was developed for a number of applications, including induction coil liners and molten metal transport. For more information contact Zircar on USA: +1914 651 1515 (fax).

Author
Un-named
Origin
Unknown
Journal Title
Glass 78 1 Feb/2001 44
Sector
Refractories
Class
R 383

Request article (free for British Glass members)

Mouldable Refractory Sheet
Glass 78 1 Feb/2001 44
R 383
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.