Mossbauer Spectra Of Binary Iron Oxide Based Glasses At Liquid Nitrogen Temperature

Mossbauer measurements were carried out at liquid nitrogen temperature for 40Sr0.60Fe2O3, 60Ba0.40Fe2O3 and 70Fe2O3.30P2O5 glasses prepared by the twin roller method in order to evaluate magnetic properties as well as chemical structure of these materials.

Author
K Tanaka Et Al
Origin
Kyoto University, Japan
Journal Title
Phys Chem Glasses 36 6 1995 244-246