Monitoring Trends At The Hot End

AGR International has formed an agreement with Jorgen Laessoe Ingeniofirma aps of Soborg, Denmark, to produce and market the Hot End Trend Analyzer for the glass container industry. the agreement between the two companies includes worldwide manufacturing, distribution, service and support of the Hot End Trend Analyzer by AGR, as well as future joint development work and a coordinated system enhancement effort.