Monitoring The Stressed State Of Structural Glass Blocks

Based on a polariscope/polarimeter, a device for monitoring residual stresses in structural glass blocks is developed that makes it possible to automate the measurement of residual stresses and eliminate the negative effect of the light diffusing glass block coating on the interference pattern of the residual-stress distribution in assessing the stressed state of glass articles using the polarization-optical method.

Author
A G Filatov
Origin
Unknown
Journal Title
Glass & Ceramics 57 11-12 2000 367-369