Monitoring Forehearth Temperatures

Accurate, reliable and stable temperature measurement is essential in the forehearth and working end of a glass melting tank, to ensure optimum product quality. Radiation thermometers are ideally suited to the needs of the glass industry when used to measure the temperature of molten glass.