Moisture Attack On Museum Glass Measured By Sims

Low energy secondary ion mass spectrometry (LE-SIMS) was used to measure Na and other elemental concentrations as a function of depth in a replica glass aged in humidities of 30 & 39% RH at 25 deg C. The ageing times varied from one up to 45 days. The replica glass was based on the composition of a severely corroded museum artefact, and had a high soda and low lime content. The Na depth profiles displayed a characteristic S-shape and the depth of the Na depletion increased with increasing ageing time. It was found that the increased in Na depletion followed the time relationship, indicating a diffusion controlled process. After an ageing period of 45 days the rate of formation of the depletion layer was measured to be 0.06 and 0.26nmh-1 for 30 and 39% respectively.

Author
S Fearn Et Al
Origin
Imperial College, London
Journal Title
Phys Chem Glasses 46 5 2005 505-511
Sector
Special Glass
Class
S 3046

Request article (free for British Glass members)

Moisture Attack On Museum Glass Measured By Sims
Phys Chem Glasses 46 5 2005 505-511
S 3046
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.