Modern Windows

Thermal transport in windows caused by conduction/convection and by radiation is discussed in this article. The reduction of thermal losses achieved by using rare gases and low emissivity coatings is quantified. The saving potential of evacuated window systems is also demonstrated. Furthermore, a variety of daylighting and light switching systems fitted into glazing elements are represented. The properties, applications and energy saving potentials of such elements are described.

Author
J Fricke & A Beck
Origin
Bavarian Centre Of Applied Energy Research, Wurzberg, Germany
Journal Title
Trans Indian Ceram Soc 55 2 March-April 1996 31-34
Sector
Flat glass
Class
F 764

Request article (free for British Glass members)

Modern Windows
Trans Indian Ceram Soc 55 2 March-April 1996 31-34
F 764
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.