Modern Glazing Systems

The use of coated glass products for solar gain control and increased thermal resistance has enabled the development of glazing and window products suited to application and climate. Such glazing systems may reduce building energy consumption, improve visual and thermal comfort and lessen adverse environmental impacts. This paper provides a brief overview of some important glazing materials, in particular silver-based solar control coatings and dynamic electrochromic devices, and examines relevant work undertaken within selected projects of the EU JOULE and Standards, Measurement & Testing Programmes, relevant to the area of glazing development and characterization.

Author
M G Hutchins
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 31 1 2001 5-11
Sector
Flat glass
Class
F 1222

Request article (free for British Glass members)

Modern Glazing Systems
Riv Staz Sper Vetro 31 1 2001 5-11
F 1222
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.