Modelling Of The Pressing Process In Glass Stemware Production: Computation Of Stresses For The Prediction Of Mould Damage

Glass pressing processes require a high quality inner mould surface during each production cycle and thus preventing mould wear is important in reducing costs. Thermally induced stresses are one of the phenomena that can result in mould damage. A finite element method model of a stem pressing process was developed as a tool for optimisation of the pressing process. The working cycle of a sixteen position pressing machine was simulated. Both glass and forming tools were included in the model. The calculated temperatures were validated successfully by experimental measurements. Equivalent von Mises stresses were calculated for the mould surface and those locations where the yield point of the mould material was exceeded were identified. The calculated critical locations correspond very well with those regions suffering damage in actual moulds.

Author
P Vrabel Et Al
Origin
Rona, Slovak Republic
Journal Title
Glass Technology 46 4 2005 292-297
Sector
Domestic glass
Class
D 901

Request article (free for British Glass members)

Modelling Of The Pressing Process In Glass Stemware Production: Computation Of Stresses For The Prediction Of Mould Damage
Glass Technology 46 4 2005 292-297
D 901
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.