Modelling The Evaporation Of Boron Species. Part 1: Alkali-Free Borosilicate Glass Melts

A laboratory test facility has been used to measure the boron evaporation rates from borosilicate glass melts. The impact of furnace atmosphere composition and glass melt composition on the temperature dependent boron evaporation rates has been investigated experimentally. In Part 2 of this paper the results for alkali-free borosilicate glass melts are discussed. From the measured boron evaporation rates, information on the chemical activity of B2O3 in the melt (at the glass melt surface) has been derived and compared with results of thermodynamic modelling. For alkali-free borosilicate melts, a modified thermodynamic associated species model is presented. Furthermore, the transport of volatile boron compounds in these melts are discussed. In Part 2 of this paper, the impact of the glass composition and glass structure on the boron evaporation rates ill be discussed.

Author
H Limpt Et Al
Origin
Tno, The Netherlands
Journal Title
Glass Technology 52 3 2011 77-87
Sector
Special Glass
Class
S 3928

Request article (free for British Glass members)

Modelling The Evaporation Of Boron Species. Part 1: Alkali-Free Borosilicate Glass Melts
Glass Technology 52 3 2011 77-87
S 3928
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.