Modeling Of Glass Melting Process In Plasma-Fired Skull Furnace

The present paper describes an overview of mathematical modelling of the glass melting process inside an open-top skull furnace having DC plasma discharge as the primary energy source. This melting system has been developed by Plasmelt Glass Technologies LLC (Boulder, CO, USA). A mathematical model of intensive glass melting, which is a non stationary state process, and corresponding software have been developed by a modelling team of Laboratory Glass Properties LLC (LGP). This mathematic model has been created in parallel with the development of the melting process itself. Having a fully operational pilot unit available from the Plasmelt team had the possibility to compare behaviour of a real melting system with that with that calculated by the model .

Author
Oleg. A. Prokhorenko
Origin
Laboratory Of Glass Properties, St Petersburg, Russia.
Journal Title
Advanced Materials Research Vols 39-40 (2008) 485-488
Sector
General
Class
G 3524a

Request article (free for British Glass members)

Modeling Of Glass Melting Process In Plasma-Fired Skull Furnace
Advanced Materials Research Vols 39-40 (2008) 485-488
G 3524a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.