A Model Of The Structure Of Simple Phosphate Glasses

Evaluation of the infrared absorbence spectra of several series of ultraphosphate glasses by principal component analysis was improved using a unique measure of the number of the principal components for the four systems. Three principal components are obtained even for the system of calcium and the model of the formation of the structure of the phosphate glasses by the substructures of crystalline, congruent melting ultraphosphates and metaphosphates is confirmed. But the model is not valid for vitreous P205 as before. Here a contrary model is used to explain the experimental results. It is a random network concerning the distribution of cations and PO4 tetrahedra.

Author
K Meyer
Origin
Friedrich Schiller University, Jena, Germany
Journal Title
Phys Chem Glasses 43 2 2002 108-118
Sector
Special Glass
Class
S 2382

Request article (free for British Glass members)

A Model Of The Structure Of Simple Phosphate Glasses
Phys Chem Glasses 43 2 2002 108-118
S 2382
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.