A Model Of Structural Relaxation In Glass

Study of the time dependence of physical properties in the transformation range of glass is complicated by the "memory effect" and the inherent nonlinearity which are characteristic of structural relaxation. A multiparameter model of structural relaxation is presented that differs from earlier models in that it takes account of both these effects. The model fits avilable experimental data well; these data were obtained for the most part by observing the evolution of properties (such as density or refractive index) following a step change in temperature. This model also permits prediction of the physical properties of glass subjected to arbitrary and more complex temperture-time histories. It should, therefore, also be useful in the rational design of heat treating processes such as annealing.

Author
O S Narayanaswamy
Origin
Ford Motor Co, Usa
Journal Title
Jacs 54 10 1971 491-498
Sector
Primary Papers
Class
PP 4

Request article (free for British Glass members)

A Model Of Structural Relaxation In Glass
Jacs 54 10 1971 491-498
PP 4
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.