Model Based Process Optimisation

In this paper the authors explain how TNO developed an evaporation model to predict and explain the sodium evaporation rates in different soda-lime glass furnaces.

Author
Hans Van Limpt Et Al
Origin
Tno, The Netherlands
Journal Title
Glass Int May/June 2003 34-35
Sector
General
Class
G 2632